EN 10025-5 S235J2W Atmospheric Corrosion Resistance Steel Plate

EN 10025-5 S235J2W Atmospheric Corrosion Resistance Steel Plate

EN 10025-5 S235J2W atmospheric corrosion resistance steel plate grade is a hot rolled products of structural steels in technical delivery conditions with improved atmospheric corrosion resistance.
Sende bookingforespørsel
Beskrivelse
Tekniske parametere

 

EN 10025-5 S235J2W atmospheric corrosion resistance steel plate grade is a hot rolled products of structural steels in technical delivery conditions with improved atmospheric corrosion resistance.

 

S mean S235J2W grade could be used in structural steel projects, 235 is the min yield strength.

 

J0 ,J2 and K2 standard for the impact℃and energy in 0 temperature.

 

W means that the mainly different in their carbon and phosphorus contents and availability.

 

product-431-431

For the steel grade in S235 a maximum carbon equivalent value of 0.44% and for grade s355 a maximum carbon equivalent value of 0.52% based on the ladle analysis shall for all thickness.

 

 

S355J0W

Thickness 8mm-300mm, Width: 1500-4020mm, Length: 3000-27000mm

EN10155 Technical delivery conditions for general structural steels

 

Chemical composition % of the Product analysis of grade S355J0W

 

C

P

S

N

0.19

0.55

0.45-1.60

0.20-0.60

0.040

0.040

0.35-0.85

0.010

 

Mechanical properties of grade S355J0W

 

-20

-10

0

20

Notch impact test. Min. absorbed energy J

   

27

 

 

to 16

16 - 40

40 - 63

63 - 80

80 - 100

100 - 150

ReH - Minimum yield strength (MPa)

355

345

335

325

315

295

 

to 3

3 - 100

100-150

Rm -Tensile strength (MPa)

510-680

470-630

450-600

 

>=1.5<2

>=2﹤2.5

>=2.5<3

>=3<40

>=40﹤63

>=6﹤100

>=100﹤150

A - Minimum elongation Lo=5,65 √ So (%) Longitudinal

16

17

18

22

21

20

18

 

Equivalent grades of grade S355J0W

 

EU 155

NFA35-502

WBL 087

U.K.

BS 4360

JIS G3114

Fe510 C2K1

E 36WB 3

 

WR50B

SMA 50AW

A588 Gr. A

 

 

EN10155 S235J2W steel (S235J2W steel plate) boasts excellent weather resistance and good processing performance, making it versatile for a wide range of applications.

 

Bridge Construction: S235J2W steel plate can serve as the primary construction material for bridges, withstanding corrosion in harsh climatic conditions and ensuring structural safety and service life of the bridges. Specifically, it can be used to manufacture structural components such as bridge beams, arches, and joints.

 

Road and Railway: In road and railway construction, S235J2W steel plate is used to manufacture structural components such as guardrails and roadbeds, enhancing the durability and safety of road facilities.

 

Port Facilities: Given their long-term exposure to marine environments, port facilities benefit from the weather resistance of S235J2W steel plate, making it an ideal material for manufacturing port machinery and dock facilities.

 

Equipment Manufacturing: In industries such as power, petroleum, and chemicals, S235J2W steel plate is used to manufacture corrosion-resistant equipment and structural components, ensuring stable operation of equipment in harsh environments.

 

Building Structures: S235J2W steel plate is also commonly used to manufacture structural components of buildings such as beams, columns, and plates. Its good weather resistance and processing performance effectively extend the service life of buildings.

 

Furthermore, due to its good impact toughness, S235J2W steel plate is applied in fields such as shipbuilding and vehicle manufacturing, including the manufacture of hull structural components (such as hull plates, decks, and bulkheads) and structural components of vehicle chassis, frames, and carriages. Additionally, it can be used to manufacture various mechanical parts, such as gears, bearing housings, and machine frames.

 

Contact now to get S235J2W Quote

 

product-612-706

 

Q: What is S235J2 material equivalent to?

A: EN10025 S235J2 is a carbon steel grade with good structural properties. Some common equivalent materials for EN10025 S235J2 carbon steel plate include: ASTM A36: A widely used structural steel in the U.S. that has similar properties in terms of tensile strength and yield strength.

Q: What is S235J2W steel application?

A: As steel with improved atmosphere corrosion resistance, S235J2W steel has a wide range of applications, architecture, smokestacks, freight wagons, silos, pylons, bridges etc.

删除

 

Populære tags: en 10025-5 s235j2w atmospheric corrosion resistance steel plate, China en 10025-5 s235j2w atmospheric corrosion resistance steel plate manufacturers, suppliers